230 Casting System Model casting Stand 1.9. 03 A 25
3. Finishing of titanium castings
Safety advices!
Abraded or separated titanium particles when
hot react with oxygen and produce sparks.
Caution: Risk of combustion and explosion.
Cool the workpiece with water.
If suction lines are used, change the filter paper
regularly. Warning: Otherwise fire hazard.
Warning! Always use trimming materials only for
processing titanium. Keep separate!
Cutting of sprues
Warning! Do not overheat the casting when separating.
Cool. No red heat.
For recommended separating discs, see page C 6.
Grinding
If possible, use carbide burs and trim in one direction.
Tungsten carbide burs are particularly suitable (see page C 6).
Grinding points can be used for smoothing surfaces
(see page C 6).
Note! Use carbide burs and grinding points only for
trimming rematitan
®
. Keep separate!
Preparation for ceramic bonding
Surfaces which are to be blended with ceramic must be
finished entirely with carbide burs. The amount of material
removed depends on the particular material thickness.
Afterwards, blast off the framework surface with aluminum
oxide and condition according to the ceramic manufacturer’s
instructions.
Rubber polishing
When rubber polishing, it is essential to avoid severe
heating of the polishing surfaces!
(For recommended rubber polishers, see page C 6.)
Uniform smoothing of the metal surface to be polished is
achieved if this has been ground with very fine emery paper
(500 1000 grain) in a sandpaper holder.
Acid treatment
Do not place titanium castings in hydrofluoric acid.
Titanium is quickly damaged by hydrofluoric acid!
Danger